年级 | C | 锰 | P | S | 硅 | Cr | 你 | 莫 | N | 其他 |
316 | ≤0.08 | ≤2.0 | ≤0.045 | ≤0.03 | ≤1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | – | – |
316L | ≤0.035 | ≤2.0 | ≤0.045 | ≤0.03 | ≤1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | – | – |
316H | 0.04-0.10 | ≤2.0 | ≤0.045 | ≤0.03 | ≤1.0 | 16.0-18.0 | 11.0-14.0 | 2.0-3.0 | – | – |
316钛 | ≤0.08 | ≤2.0 | ≤0.045 | ≤0.015 | ≤0.75 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | ≤0.1 | 钛:5×(C%+N)-0.7 |
316N | ≤0.08 | ≤2.0 | ≤0.045 | ≤0.03 | ≤2.0 | 16.0-18.0 | 10.0-13.0 | 2.0-3.0 | 0.1-0.16 | – |
316LN | ≤0.035 | ≤2.0 | ≤0.045 | ≤0.015 | ≤0.015 | 16.0-18.0 | 10.0-13.0 | 2.0-2.5 | 0.1-0.16 | – |
年级 | 抗拉强度 ksi(兆帕) | 屈服强度 ksi(兆帕) | 伸长,% | 硬度 布氏/维氏 | 硬度 罗克韦尔 |
316 | ≥75(515) | ≥30(205) | ≥35 | ≤192HBW/200HV | ≤90HRB |
316L | ≥70(485) | ≥25(170) | ≥35 | ≤192HBW/200HV | ≤90HRB |
316H | ≥75(515) | ≥30(205) | ≥35 | ≤192HBW/200HV | ≤90HRB |
316钛 | ≥75(515) | ≥30(205) | ≥35 | ≤192HBW/200HV | ≤90HRB |
316N | ≥80(550) | ≥35(240) | ≥35 | ≤192HBW/200HV | ≤90HRB |
· 食品加工设备 啤酒设备、
· 化工石化设备、
· 实验台及设备
· 海滩甲板覆盖物,
· 海岸线覆盖,
· 船用紧固件、
· 化学品容器、
· 热交换器、
· 矿用筛、
· 弹簧,
· 医疗植入物。
TP316Ti /1.4571/UNSS31635 是一种钛稳定的钼合金奥氏体铬镍合金三通l,具有改进的机械加工性能,具有与 AISI 316L 相似的特性,但 TP 316Ti 具有更好的机械性能和高温强度。TP 316Ti(1.4571,UNS S31635)由于添加了钛而表现出更高的耐腐蚀性。
通常考虑使用 TP 316Ti(1.4571,UNS S31635),但不耐热海水。热氯化物环境可能会导致点蚀和缝隙腐蚀。TP 316Ti(1.4571,UNS S31635)耐热性316在870℃和925℃的温度下连续使用时表现出良好的抗氧化性。但是,如果需要耐水腐蚀,则在425-860℃下连续使用°C 不推荐。在这种情况下,由于耐碳化物析出,建议使用 316L。当需要500℃以上高温时,建议使用316H级。